CHEMICAL COMPOSITIONE
incoloy 625 plexum capillarium Tubing
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0.5 | ≤ 0.5 | 8 – 10 | ≤ I * | ≤ 0.014 | ≤ 0.014 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(massa %)
* Si determinari
ASTM B444, ASME SB444, AMS 5581
Per ASTM B444, ASME SB444, AMS 5581
Conditio | Distrahentes fortitudo | Cedat imperium | Prolongatio |
minimum, ksi | minimum, ksi | minimum, % | |
Gradus 1 | 120 | 60 | 30 |
Gradus 2 | 100 | 40 | 30 |
Superiores vires possessiones in frigore obdurato provideri possunt.
incoloy 625 plexum capillarium Tubing
70°F | 200°F | 400°F | DC°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Density | libras / in3 | 0.305 | - | - | - | - | - |
Scelerisque Expansion | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Modulus elasticus | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Ratio Poisson | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Scelerisque conductivity | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Imprimis Caloris | Btu/lb·°F | 0.093 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Cedat imperium | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Distrahentes fortitudo | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 plexum capillarium Tubing
PROCESSDESCRIPTIONSteel MakingElectric Arcus Fornax sequitur Vacuum Oxygeni Decarburizationis (VOD) vel Argon Oxygeni Decarburizationis (AOD). Pipe MakingConventional Seamless Frigidum Finitum Pipe et Tube Vestibulum Processes. Tractatio Caloris curatio caloris indurari non potest.Praeberi in annealed, solutione annata vel frigida conditione indurata.Superior vis annata conditio in servitiis ad 1100°F typice adhibita est, cum solutione annata condicio adhibeatur in applicationibus supra MC°F.