Super Alloy HASTELLOY(r) C276 (UNS N10276) 6.35*1.65 mm
Compositio chemica
Super Alloy HASTELLOY(r) C276 (UNS N10276) 6.35*1.65 mm
Compositio chemica HASTELLOY (r) C276 in sequenti tabula delineatur.
Elementum | Content (%) |
---|---|
Nickel, Ni | 57 |
Molybdenum, Mo | 15-17 |
Chromium, Cr | 14.5-16.5 |
Ferrum, Fe | 4-7 |
Wolframium, W | 3-4.50 |
Cobalt, Co | 2.50 |
Manganum | 1 |
Vanadium, V | 0.35 |
Pii, Si | 0.093 |
Phosphorus, P | 0.024 |
Carbon, C | 0.011 |
Sulphur, S | 0.011 |
Corporalia Properties
Super Alloy HASTELLOY(r) C276 (UNS N10276) 6.35*1.65 mm
Sequens tabula ostendit proprietates physicas HASTELLOY(r) C276.
Properties | Metric | Imperiale |
---|---|---|
Density | 8.89 g/cm³ | 0.321 lb/in³ |
Liquescens punctum | 1371°C | 2500°F |
Mechanica Properties
Super Alloy HASTELLOY(r) C276 (UNS N10276) 6.35*1.65 mm
Mechanica HASTELLOY(r) C276 in sequenti tabula exhibentur.
Properties | Metric | Imperiale |
---|---|---|
Robur distrahens (@ crassitudo 4.80-25.4 mm, 538°C/@ crassitudo 0.189-1.00 in, 1000°F) | 601.2 MPa | 87200 psi |
Cedant vires (0.2% offset, @ grossitudo 2.40 mm, 427°C/@ grossitudo 0.0945 in, 801°F) | 204.8 MPa | 29700 psi |
Modulus elasticus (RT) | 205 GPa | 29700 ksi |
Prolongatio ad intermissum (in 50.8 mm, @ grossitudo 1.60-4.70 mm, 204°C/@ grossitudo 0.0630-0.185 in, 399°F) | 56% | 56% |
Duritia, Rockwell B (plate) | 87 | 87 |
Scelerisque Properties
Proprietates thermarum de HASTELLOY C276 traduntur in tabula sequenti.
Properties | Metric | Imperiale |
---|---|---|
Scelerisque dilatatio co-efficiens (@24-93°C/75.2-199°F) | 11.2 µm/m°C | 6.22 µin/in°F |
Scelerisque conductivity (-168 °C) | 7.20 W/mK | 50.0 BTU in/hr.ft².°F |
Aliae Vocabula
Equivalent materials to HASTELLOY(r) C276 haec sunt.
ASTM B366 | ASTM B574 | ASTM B622 | ASTM F467 | DIN 2.4819 |
ASTM B575 | ASTM B626 | ASTM B619 | ASTM F468 | |